MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Trinseo TYRIL™ 790 Styrene-Acrylonitrile
Categories: Polymer; Thermoplastic; SAN Polymer

Material Notes: TYRIL™ styrene-acrylonitrile (SAN) resins are designed to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications. The key property of TYRIL 790 is its high flow that results in excellent processability. TYRIL 790 is specifically designed for end-use applications requiring a good balance of physical properties, optical properties (gloss, clarity or opaqueness), heat resistance and practical toughness.

Applications:

  • Tableware: airline serviceware, other multi-cavity applications
  • Personal care: combs, toothbrushes
  • Electronics: dust covers, display screens
Complies with:
  • Europe Food-Contact Compliance
  • FDA, 21 CFR.177.1640.

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
Apparent Bulk Density 0.690 g/ccISO 60
Melt Flow 9.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 21 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 84ASTM D785
Tensile Strength at Break 72.0 MPa5 mm/min; ASTM D638
 72.0 MPaISO 527-2/5
Tensile Modulus 3800 MPaISO 527-2/5
Flexural Strength 118 MPaASTM D790
Izod Impact, Unnotched (ISO) 13.0 kJ/m²ISO 180
Charpy Impact Unnotched 16.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 9.10 kV/mmIEC 60243-1
Dissipation Factor 0.00010
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°CDIN 53752
Specific Heat Capacity 1.38 J/g-°CASTM D2766
Deflection Temperature at 1.8 MPa (264 psi) 101 °CAnnealed; ISO 75-2/A
Vicat Softening Point 101 °CISO 306/B50
 110 °CISO 306/A120
Flammability, UL94 HB
@Thickness 1.60 mm
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo TYRIL™ 905 Styrene-Acrylonitrile

PTRINS9098 / 197571

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.