GD5150K is a high-density polyethylene specially developed for the manufacturing of insulation for wires and cables demanding high extrusion velocity. It has medium molar mass, shows good dielectric properties, and contains special additives to prevent catalytic oxidation of copper. Its applications include insulation for wires and cables and multiplex cables. |