MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Silicone Polyurethane, Ether Based
Categories: Polymer; Thermoplastic; Polyurethane, TP; Silicone Polyurethane, Ether Based

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.978 - 1.11 g/ccAverage value: 1.05 g/cc Grade Count:9
Molecular Weight 95000 g/molAverage value: 95000 g/mol Grade Count:4
Linear Mold Shrinkage 0.0110 - 0.0360 cm/cmAverage value: 0.0204 cm/cm Grade Count:5
Linear Mold Shrinkage, Transverse 0.00800 - 0.0230 cm/cmAverage value: 0.0148 cm/cm Grade Count:3
Melt Flow 2.00 - 37.0 g/10 minAverage value: 21.2 g/10 min Grade Count:5
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55.0 - 95.0Average value: 76.1 Grade Count:15
Hardness, Shore D 50.0 - 80.0Average value: 65.1 Grade Count:7
Tensile Strength, Ultimate 12.0 - 60.0 MPaAverage value: 29.8 MPa Grade Count:22
Elongation at Break 25.0 - 823 %Average value: 453 % Grade Count:22
Modulus of Elasticity 0.00800 - 0.750 GPaAverage value: 0.188 GPa Grade Count:12
Flexural Yield Strength 1.45 - 1.86 MPaAverage value: 1.61 MPa Grade Count:3
Flexural Modulus 0.0371 - 0.0433 GPaAverage value: 0.0396 GPa Grade Count:3
Tear Strength 20.2 - 175 kN/mAverage value: 72.6 kN/m Grade Count:19
Taber Abrasion, mg/1000 Cycles 5.40 - 85.0Average value: 29.7 Grade Count:5
Compression Set 15.0 - 29.0 %Average value: 21.7 % Grade Count:9
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.70 - 7.00Average value: 6.28 Grade Count:5
Dielectric Strength 11.8 - 16.5 kV/mmAverage value: 13.7 kV/mm Grade Count:5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 187 - 200 µm/m-°CAverage value: 192 µm/m-°C Grade Count:5
Vicat Softening Point 67.0 - 82.0 °CAverage value: 74.0 °C Grade Count:3
Glass Transition Temp, Tg -68.0 - -12.0 °CAverage value: -35.7 °C Grade Count:3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 182 - 204 °CAverage value: 193 °C Grade Count:5
Drying Temperature 82.0 - 104 °CAverage value: 93.0 °C Grade Count:3
Moisture Content 0.0100 %Average value: 0.0100 % Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
Overview of materials for Silicone Polyurethane, Polycarbonate Based
Overview of materials for Silicone Rubber

O5050 / 78467

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.