MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Embrace Shrink Film Extruded/Cast  (discontinued **)
Categories: Polymer; Film; Thermoplastic

Material Notes: Embrace shrink film is the world’s leading shrink film for dairy, water, juice, liquor, and sports and soft drink beverage packaging. Embrace shrink film provides excellent clarity, printability, and toughness, enabling marketers to increase shelf visibility, presence, and appeal for their products. With ultimate shrinkage of over 80%, Embrace shrink film is the ideal label material for marketers looking to differentiate their products in the competitive beverage market.

Applications/Uses

  • Labels to fit high contour containers
  • Super-high print definition
  • Wrap around design
  • Key Attributes

  • Good chemical resistance
  • Good gloss and sparkle
  • High shrink force
  • Excellent clarity
  • Greater than 80% ultimate shrinkage
  • Shrinks to fit contour bottles
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.30 g/ccASTM D1505
    Water Vapor Transmission 7.60 g/m²/dayASTM F372
    Oxygen Transmission 23.0 cc-mm/m²-24hr-atmASTM D3985
    Viscosity Measurement 0.70Inherent; EMN-A-AC-G-V-1
    Thickness 250 micronsASTM D374
     
    Mechanical PropertiesOriginal ValueComments
    Film Elongation at Break, MD 5.0 %ASTM D882
    Film Elongation at Break, TD 5.0 %ASTM D882
    Tensile Modulus 1.56 GPaTD; ASTM D882
     1.57 GPaMD; ASTM D882
    Tear Strength, Total 15.7 NSplit Tear Method, 254mm/min, TD; ASTM D1938
     15.7 NSplit Tear Method, 254mm/min, MD; ASTM D1938
     61.0 NPPT Tear Resistance, MD; ASTM D2582
     66.0 NPPT Tear Resistance, TD; ASTM D2582
    Elmendorf Tear Strength, MD 3.04 g/micronASTM D1922
    Elmendorf Tear Strength, TD 3.04 g/micronASTM D1922
    Dart Drop 1.42 g/micronASTM D1709A
    Film Tensile Strength at Break, MD 53.0 MPaASTM D882
    Film Tensile Strength at Break, TD 53.0 MPaASTM D882
     
    Thermal PropertiesOriginal ValueComments
    Vicat Softening Point 74.0 °C1kg load; ASTM D1525
    Glass Transition Temp, Tg 75.0 °CASTM D3418
     
    Optical PropertiesOriginal ValueComments
    Haze 0.70 %ASTM D1003
    Gloss 166 %at 60°; ASTM D2457
    Transmission, Visible 67 %Transparency; ASTM D1746
     89 %Regular Transmittance; ASTM D1003
     92 %Total Transmittance; ASTM D1003

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    PE9074 / 35130

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.