MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 El Mar® 3000 Oil SAE Grade 40
Categories: Fluid; Lubricant

Material Notes: Description: Conoco El Mar® 3000 Oil is a quality, low ash gas engine oil recommended for naturally aspirated and moderately turbocharged, four cycle, low-, medium- and high-speed gas engines, such as Caterpillar*; Cooper-Superior (formerly White-Superior); Waukesha; Navistar (formerly International Harvester); Dresser-Rand (formerly Ingersoll-Rand) Category I, II and III; Minneapolis Moline; Onan and Detroit Diesel (gas or dual-fuel conversion). El Mar 3000 Oil is formulated with high-viscosity index base oils blended with selected additives and a unique ashless dispersant to provide good resistance to oxidation and nitration, reduced carbon-forming tendencies, good piston ring groove and crankcase cleanliness and ring and liner protection. Highly loaded engines (>80 percent) and/or engines operated with extended lubricant drain intervals may build engine deposits, which may become excessive. If operating under these extreme conditions, Hydroclear El Mar LA4 is recommended. Remote engines operated intermittently or in cold weather benefit from the low temperature pumpability provided by the SAE 15W-40 viscosity grade.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.884 g/cc
@Temperature 15.6 °C
Density 7.36 lb/gal
API Gravity 28.6 °
Viscosity Measurement 93Viscosity Index
Kinematic Viscosity at 40°C (104°F) 124 cSt
Kinematic Viscosity at 100°C (212°F) 13 cSt
Ash 0.41 %Sulfated Ash
ASTM Color 3.5
 
Chemical PropertiesOriginal ValueComments
Total Base Number 5.1
 
Thermal PropertiesOriginal ValueComments
Pour Point 16.0 °F
Flash Point 495 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco 17 SG 2000 Diesel Engine Oil
ChevronTexaco 17 MG 2000 Diesel Engine Oil
ChevronTexaco 13 SG Diesel Engine Oil
ChevronTexaco DIESELMOTIVE® Direct Injector Cleaner, for Heavy Duty Diesel Engines
ChevronTexaco Delo® 100 Motor Oil, SAE 30

WCON244 / 75281

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.