MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

ITW Devcon Plastic Welder™ Methacrylate Adhesive II, Ultra White
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes:

Information provided by ITW Devcon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 56000 cP56000 cPMixed Viscosity (Thixotropic gel)
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 5.0 - 15 %5.0 - 15 %
Adhesive Bond Strength 20.7 MPa3000 psilap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002
Tensile Impact Strength 35.7 kJ/m²17.0 ft-lb/in²
Peel Strength 2.63 - 3.51 kN/m15.0 - 20.0 pli
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °Fdry
Minimum Service Temperature, Air -55.0 °C-67.0 °Fdry
 
Processing PropertiesMetricEnglishComments
Cure Time 8.00 - 10.0 min0.133 - 0.167 hourFixture time
 120 - 240 min2.00 - 4.00 hourFunctional cure
Working Life 2.00 - 3.00 min2.00 - 3.00 min
 
Descriptive Properties
Mix ratio (Resin:Hardener)1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITW13 / 48462

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.