MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

UNS C81500, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Investment, Permanent Mold, Plaster, and Sand.

Applications: Electrical and/or thermal conductors used as structural members where strength and hardness greater than that of UNS C8100-8110 are required.

Mechanical properties typical for sand cast test bars, heat treated.

Key Words: chromium copper, chrome copper, CA 815
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.82 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 105105
Tensile Strength, Ultimate 350 MPa50800 psi
Tensile Strength, Yield 275 MPa39900 psi
Elongation at Break 17 %17 %in 50 mm
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.320.32
Fatigue Strength 105 MPa
@# of Cycles 1.00e+8
15200 psi
@# of Cycles 1.00e+8
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
Izod Impact 41.0 J30.2 ft-lb
Charpy Impact 27.0 J19.9 ft-lbV-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000210 ohm-cm0.00000210 ohm-cmPrecipitation hardened
 0.00000383 ohm-cm0.00000383 ohm-cmSolution heat treated
Magnetic Permeability 1.01.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.1 µm/m-°C
@Temperature 20.0 - 300 °C
9.50 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.376 J/g-°C0.0899 BTU/lb-°F
Thermal Conductivity 315 W/m-K
@Temperature 20.0 °C
2190 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1075 - 1085 °C1967 - 1985 °F
Solidus 1075 °C1967 °F
Liquidus 1085 °C1985 °F
Shrinkage 2.1 %2.1 %Patternmaker's Shrinkage (1/4 in./ft.)
 
Processing PropertiesMetricEnglishComments
Solution Temperature 1000 - 1010 °C1830 - 1850 °F
Aging Temperature 480 °C896 °F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 0.40 - 1.5 %0.40 - 1.5 %
Copper, Cu 98 - 99.6 %98 - 99.6 %
Lead, Pb <= 0.015 %<= 0.015 %
Other, total <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.040 %<= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
UNS C81400, Copper Casting Alloy
UNS C80100, Copper Casting Alloy
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper
UNS C81700, Copper Casting Alloy
MetalTek Copper Ni Si Cast UNS C81540 High Conductivity

MC81500b1 / 11859

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.