MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chosun Refractories TG-68 Monolithic Refractories for Ladle and Tundish
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.003924 GPa
@Temperature 1500 °C,
Time 10800 sec
0.5691 ksi
@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 9.81 MPa
@Treatment Temp. 1500 °C,
Time 10800 sec
1420 psi
@Treatment Temp. 2730 °F,
Time 3.00 hour
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Shrinkage  -0.350 %
@Temperature 1500 °C,
Time 10800 sec
-0.350 %
@Temperature 2730 °F,
Time 3.00 hour
 -0.0500 %
@Temperature 110 °C,
Time 86400 sec
-0.0500 %
@Temperature 230 °F,
Time 24.0 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 65 %65 %
SiO2 27 %27 %
 
Descriptive Properties
Installation MethodGunnung, Troweling
Main ApplicationsTundish Coating
Material Required for Estimating (kg/m3)2,000
Water Required for Casting(%)NOZZLE Mixing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CCHOS294 / 124238

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.