Product Description: PPH005 is a fractional melt flow polypropylene homopolymer resin available in pellet form and is made with non-phthalate catalyst. Typical applications include raffia/tapes/strapping, anti-corrosion coating, geotextile and agriculture and nets. Availability: North America Features: Good Flow; Homopolymer Uses: Agricultural Applications; Coating Applications; Netting; Strapping; Tape Forms: Pellets Information provided by Osterman & Company |