MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay MACKADET® EQ-178 Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Product Description: Mackadet EQ-178 is a mild, concentrated blend of surfactants for use as a base for high foam personal care products. This blend is free of alcohol, diethanolamides, lauryl sulfates, laureth sulfates, parabens and formaldehyde. The surfactant ingredients in this blend are all derived from natural, renewable resources. Mackadet EQ-178 responds gently to viscosity building with the simple addition of sodium chloride. This grade is preserved with Kathon® CG-ICP.

Uses: Shampoos, Body Washes and Hand Soaps

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/cc
Solids Content 42 - 45 %Moisture Balance
pH 6.0 - 7.510% Aqueous
Viscosity 1000 cP8% Solid, 0.5% NaCl
 2000 cP8% Solid, 1.5% NaCl
 3000 cP10% Solid, 0.5% NaCl
 4000 cP10% Solid, 1.5% NaCl
 5000 cP12% Solid, 0.5% NaCl
 5900 cP12% Solid, 1.5% NaCl
 <= 7000 cP#3 SP @ 12 rpm
 7200 cP14% Solid, 0.5% NaCl
 7600 cP14% Solid, 1.5% NaCl
 8400 cP15% Solid, 0.5% NaCl
 8400 cP15% Solid, 1.5% NaCl
 9400 cP16% Solid, 1.5% NaCl
 9500 cP16% Solid, 0.5% NaCl
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 4.0
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceClear to Slightly Hazy Liquid
CompositionTotal Plate Count<100 cfu/g
PreservativeMethylchloroisothiazolinone11.5 ppm
 Methylisothiazolinone3.5 ppm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay MACKADET® DR-100M Surfactant
Solvay MACKADET® EQ-112 Surfactant
Solvay MACKADET® CA-ND Surfactant
Solvay MACKADET® SBC--8 Surfactant
Verdant Specialty Solutions MACKADET® 40-K Surfactant

WRHOD191 / 137422

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.