MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow Primacor® 2912 Ethylene Acrylic Acid (EAA)
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: PRIMACOR® 2912 polymer containing 9.5% comonomer is an extrusion/ coextrusion coating resin for flexible packaging applications. It is designed to provide excellent adhesion to metallic, paper and polyethylene substrates and offers excellent slip characteristics and heat sealability. When used unmodified for food packaging applications, this resin complies with the U.S. Food, Drug and Cosmetic Act as amended under Food Additive Regulation 21 CFR 177.1310(b). This resin will also comply with 21 CFR 175.105, 176.170(b), 176.180, and 178.1005. The regulations should be consulted for complete details.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.941 g/cc
Melt Flow 12 g/10 min
@Load 2.16 kg
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 16.8 MPa
Tensile Strength, Yield 8.50 MPa
Elongation at Break 580 %
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 76.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Primacor® 3460 Ethylene Acrylic Acid (EAA)
Dow Primacor® 3150 Ethylene Acrylic Acid (EAA)
Dow Primacor® 1321 Ethylene Acrylic Acid (EAA)
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA)
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA)

PDW524 / 34593

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.