MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT ICM 1501C Silicone Antifoam
Categories: Other Engineering Material

Material Notes: Description: CHT USA's 100% active defoamers are formulated to control foam in a wide variety of industrial processes.

Key Features

  • Compound-free defoaming behavior with no deposition
  • Imparts a surface leveling effect
  • Effective at low dosage levels
  • Works in aqueous and most non-aqueous systems with some polarity
Key Applications
  • Cloud point defoamer
  • Waste water treatment
  • Coatings
  • Textiles
Application: ICM 1501C is a non ionic silicone glycol copolymer soluble in water, alcohol and hydroalcoholic systems. ICM 1501C acts as a surface tension depressant in aqueous systems and enhances pulp drainage by decreasing air entrapment. This product has been designed to improve dispersion and efficiency of defoaming agents. This product is used as an additive in paints and coatings where surface defects are not permitted.

Addition Rates
Dosage - 1: 0.1-1.0% by weight

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Storage Temperature <= 40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceTransparent liquid
ColorClear to amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL249 / 314732

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.