MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Regal® AW 100
Categories: Fluid; Lubricant

Material Notes: Texaco Regal AW oil delivers value through:
  • High Temperature stability provides long lubricant life and resistance to formation of sludge and varnish on bearings and gears.
  • Excellent wear protection provides long bearing life and protects gears from scuffing.
  • Excellent water separability provides benefits for circulating oil systems subject to severe water contamination
  • Effective foam inhibition — Reduces the amount of entrained air in the oil, minimizing the possibility of pump cavitation and also prevents surface foam.

Texaco Regal AW 100 is a circulating oil formulated from high quality base stocks and a carefully balanced, zinc-free additive package. This provides excellent protection against wear for long bearing and gear life. Texaco Regal AW 100 has superior water separability properties and rust protection to deal with the severe water contamination that frequently occurs in circulating oil systems. Its outstanding oxidation stability minimizes deposit formation and leads to long lubricant life.

Texaco Regal AW 100 is a circulating oil designed for the steel industry. It is formulated to meet the needs of circulation systems serving high speed rollers and plain bearings in no-twist finishing mills It is also recommended for the lubrication of reduction gears and bearings where zinc-free oils are desired.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 220628; MSDS Number: 8782

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 31.2 °
Viscosity Measurement 105Viscosity Index
Saybolt Viscosity at 100°F 494 SUS
Saybolt Viscosity at 210°F 65 SUS
Kinematic Viscosity at 40°C (104°F) 95 cSt
Kinematic Viscosity at 100°C (212°F) 11.3 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -15.0 °C
Flash Point 276 °C
 
Descriptive Properties
FZG Pass Stage13DIN 51354
Rust PreventionPassSSW

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WTEXA156 / 77035

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.