MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay Engineered Polymers SEQUEL® 1493 Engineered Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Description: SEQUEL® 1493 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent processability. This product is designed for pre-colored, unpainted applications.

Applications: Bumper fascias and other large components that must exhibit durable paintability or excellent weatherability.

Information provided by Solvay Engineered Polymers.

LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccISO 1183
Linear Mold Shrinkage 0.0080 cm/cmas molded; ISO 294
Melt Flow 30 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 21.5 MPa150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.565 GPa80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test >= 29.4 Jmultiaxial, 2.2 m/s; ASTM D3763

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Sequel 1493-UV LC NH696 BLK Polypropylene
LyondellBasell Sequel 1492-UV NH647 MET GD Thermoplastic Olefinic Elastomer
LyondellBasell Sequel 1493-UV NH-886M Silver Met Polyolefin
LyondellBasell Sequel 1493-UV NH533 Thermoplastic Olefinic Elastomer

PSOLE07 / 68012

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.