MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Elastocon TPE Technologies Elastocon® CLR40 Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Elastocon® CLR40 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR40 is FDA compliant and well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® CLR40 can be overmolded onto polypropylene.

Information provided by Elastocon TPE Technologies, Inc. Elastocon® TPE Technologies has been acquired by Aurora Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.025 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 43ASTM D2240
Tensile Strength 6.50 MPaASTM D412
Elongation at Break 728 %ASTM D412
100% Modulus 0.00142 GPa
@Strain 100 %
ASTM D412
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 330 - 350 °F
Front Barrel Temperature 360 - 370 °F
Nozzle Temperature 380 - 400 °F
Mold Temperature 70.0 - 100 °F
Back Pressure 100 - 200 psi
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Injection RateFast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Americas Styrenics STYRON® 666D High Heat Crystal Polystyrene
BASF Elastollan® 1185 A W TPUR
BASF Ultramid® 1403-2 BK ND3007 PA66 (Conditioned)
BASF Ultrason® E 2010 PES
Eastman Eastar GN007 PETG Copolyester

PELASC314 / 142490

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.