MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Monprene® OM-12250-01 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene OM-12250-01 is designed for overmolding applications for consumer industry. Monprene OM-12250-01 is a medium hardness, medium density, opaque grade suitable for both injection molding and extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Bondability; Light Stabilized; Low Flow; Medium Density; Medium Hardness; UV Absorbing; Without Fillers

Uses: Appliances; Bonding; Cell Phones; Flexible Grips; Handles; Knobs; Overmolding; Power/Other Tools; Sporting Goods; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  52
@Time 1.00 sec
52
@Time 0.000278 hour
Injection Molded; ASTM D2240
 60
@Time 5.00 sec
60
@Time 0.00139 hour
Injection Molded, Aged 48 hrs; ASTM D2240
 62
@Time 1.00 sec
62
@Time 0.000278 hour
Injection Molded, Aged 48 hrs; ASTM D2240
Tensile Strength at Break 7.58 MPa1100 psiDie C, 20 in/min, Flow; ASTM D412
 7.72 MPa1120 psiDie C, 20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain  1.67 MPa
@Strain 100 %
242 psi
@Strain 100 %
Die C, 20 in/min, Across Flow; ASTM D412
 2.04 MPa
@Strain 100 %
296 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
 2.88 MPa
@Strain 300 %
418 psi
@Strain 300 %
Die C, 20 in/min, Across Flow; ASTM D412
 3.30 MPa
@Strain 300 %
479 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 670 %670 %Die C, 20 in/min, Across Flow; ASTM D412
 670 %670 %Die C, 20 in/min, Flow; ASTM D412
Tear Strength 28.4 kN/m162 pliDie C, 20 in/min, Flow; ASTM D624
 30.2 kN/m172 pliDie C, 20 in/min, Across Flow; ASTM D624
Compression Set  18 %
@Temperature 22.8 °C,
Time 79200 sec
18 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 65 %
@Temperature 70.0 °C,
Time 79200 sec
65 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 193 °C320 - 380 °FMelt, Injection
Rear Barrel Temperature 160 - 193 °C320 - 380 °FInjection
Middle Barrel Temperature 160 - 193 °C320 - 380 °FInjection
Front Barrel Temperature 160 - 193 °C320 - 380 °FInjection
Nozzle Temperature 160 - 193 °C320 - 380 °FInjection
Zone 1 160 - 182 °C320 - 360 °FExtrusion
Zone 2 160 - 182 °C320 - 360 °FExtrusion
Zone 3 160 - 182 °C320 - 360 °FExtrusion
Zone 4 160 - 182 °C320 - 360 °FExtrusion
Zone 5 160 - 182 °C320 - 360 °FExtrusion
Die Temperature 160 - 182 °C320 - 360 °FExtrusion
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °FInjection
Drying Temperature 60.0 °C140 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 1.38 - 5.52 MPa200 - 800 psiInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0906 / 237397

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.