MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo INSPIRE™ TF0808S(U) Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: TF0808S(U) is a talc filled PP exhibiting high impact resistance and a high stiffness. It is particularly well suited for low wall thickness bumper skins.
  • INSPIRE TF0808S for painted parts
  • INSPIRE TF0808SU for unpainted parts with a UV stabilization package

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ISO 1183B
Filler Content 5 %5 %Talc
Linear Mold Shrinkage 0.0080 - 0.010 cm/cm0.0080 - 0.010 in/inISO 294-4
Melt Flow 17 g/10 min
@Load 2.16 kg,
Temperature 230 °C
17 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psi50mm/min; ISO 527
Elongation at Yield >= 400 %>= 400 %ISO 527
Tensile Modulus 1.20 GPa174 ksi1 mm/min; ISO 527
Flexural Modulus 1.30 GPa189 ksi3 points and 2 mm/min; ISO 178
Izod Impact, Notched (ISO) 42.0 kJ/m²20.0 ft-lb/in²ISO 180/1A
 4.00 kJ/m²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
Charpy Impact, Notched 4.50 J/cm²21.4 ft-lb/in²ISO 179-1/1eA
 0.400 J/cm²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear  63.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
35.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
DIN 53752
 93.0 µm/m-°C
@Temperature 25.0 - 80.0 °C
51.7 µin/in-°F
@Temperature 77.0 - 176 °F
DIN 53752
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FUnannealed; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FUnannealed; ISO 75
Vicat Softening Point 125 °C257 °F9.8N / 120°C / h; ISO 306 A
Shrinkage 1.0 - 1.2 %1.0 - 1.2 %ISO 294-4
 1.0 - 2.0 %1.0 - 2.0 %ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 260 °C374 - 500 °F
Mold Temperature 20.0 - 60.0 °C68.0 - 140 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2 hour2 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Buckeye Polymers BP RPP 0511C Polypropylene, 5% Mineral Filled
Buckeye Polymers BP RPP 1012 C Polypropylene, 10% Mineral Filled
Dow INSPIRE™ TF1300 Polypropylene
Tipco Tipcolene® FPC 10 - 10% Calcium Carbonate Reinforced Polypropylene Homopolymer
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade

PZZDOW1144 / 30348

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.