MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Meyors Chemical Rubber Antioxidant TMQ (RD)
Categories: Other Engineering Material

Material Notes: Product Code: MSHQD-AN025-00GT
Chemical Name: 2,2,4-trimethyl-1,2-dihydrquinoline
Trade Name: Rubber Antioxidant TMQ (RD)
CAS No.: 26780-96-1
Molecular Formula: (C12H15N) n

Typical Properties: This product in brown to amber granule, Soluble in benzene, chloroform, carbon disulfide and acetone, but not soluble in water. the toxicity is light, pollution is low, fine solution with rubber. This product is combustible, when storing and transporting, always pay attention to fireproof and damp proof

Recommended Applications: It provides oxidation protection to nearly all elastomer types in a variety of applications, having a wide range of temperatures exposure. Its long persistence in rubber allows it to provide long-term heat aging resistance to rubber compounds. It inhibits oxidation catalyzed by heavy metals such as cooper and manganese. As a result of its high molecular weight, TMQ migrates slowly within the rubber martrix and does not bloom.

Information provided by Meyors Chemical INC Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.620 - 0.650 g/cc0.0224 - 0.0235 lb/in³Compacted
Density 1.10 g/cc0.0397 lb/in³
Molecular Weight 175 g/mol175 g/mol
Ash <= 0.30 %<= 0.30 %
 
Thermal PropertiesMetricEnglishComments
Softening Point 80.0 - 100 °C176 - 212 °F
 
Descriptive Properties
AppearanceAmber or brown granule
Content<0.05%Insoluble in ethanol
 520-570 mgHCIO4/gAlkalinity index
Loss on drying<0.3%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMEYORS016 / 316598

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.