MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chemours Viton® GBL-200S Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Is ideal for blending with Viton® GBL-600S to reach intermediate viscosity ranges
  • Cures exceptionally fast to a high state of cure
  • Exhibits improved mold release/mold fouling properties compared to Viton® GBL-900 and Viton® GBL-200
  • Exhibits improved mold flow and less shear sensitivity than 65 Mooney Viton® GBL-600S
  • Exhibits excellent physical properties with high elongation, both original and aged compounds
  • Exhibits similar heat, fluids, and low temperature resistance compared to Viton® GBL-200
  • Exhibits excellent compression set resistance with little (2 hr) or no postcure either low or no postcure

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.84 g/ccUncompounded Viton
Mooney Viscosity 25
@Temperature 121 °C
ML (1+10), Uncompounded Viton; ASTM D1646
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 67No Postcure; ASTM D2240
 704 hours Postcure; ASTM D2240
Tensile Strength at Break 13.2 MPaNo Postcure; ASTM D412
 19.6 MPa4 hours Postcure; ASTM D412
Tensile Stress at Strain 0.700 MPa
@Strain 10 %
No Postcure; ASTM D412
 0.700 MPa
@Strain 10 %
4 hours Postcure; ASTM D412
Elongation at Break 289 %4 hours Postcure; ASTM D412
 319 %No Postcure; ASTM D412
100% Modulus 0.00320 GPa
@Strain 100 %
No Postcure; ASTM D412
 0.00420 GPa
@Strain 100 %
4 hours Postcure; ASTM D412
Tear Strength 10.3 kN/m
@Temperature 150 °C
Compression Set 11 %
@Temperature 200 °C,
Time 79200 sec
O-Rings, postcured; ASTM D395B
 14 %
@Temperature 200 °C,
Time 79200 sec
O-Rings, no postcure; ASTM D395B
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -18.8 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 177 °C
@Time 299 sec
Cure
 232 °C
@Time 14400 sec
Postcure
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 68 %Uncompounded Viton
 
Descriptive Properties
Coloroff-white to tanUncompounded Viton
Compound NumberA38-03
FormSheetUncompounded Viton
Formulation as Tested100GBL-200S
 2Varox® DBPH-50
 3Zinc Oxide
 3Diak 7 (TAIC)
 30MT Black
OdorNoneUncompounded Viton
Storage StabilityExcellentUncompounded Viton

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Viton® GBL-600S Fluoroelastomer Compound
Chemours Viton® GF-600S Fluoroelastomer Compound
Chemours Viton® GBLT-600S Fluoroelastomer Compound
Chemours Viton® GFLT-600S Fluoroelastomer Compound
Chemours Viton® GBLT-600S with 5-MT Black Fluoroelastomer Compound

PDVC9815 / 170456

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.