MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Tribocomp® PA66 LGF30 PTFE18 N6 Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Data for conditioned samples. MatWeb has a more thorough entry for dry samples.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 140 MPa20300 psiISO 527-2
Elongation at Break 2.8 %2.8 %ISO 527-2
Tensile Modulus 7.80 GPa1130 ksiISO 527-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 290 - 300 °C554 - 572 °F
Middle Barrel Temperature 300 °C572 °F
Front Barrel Temperature 300 °C572 °F
Nozzle Temperature 300 °C572 °F
Melt Temperature <= 300 °C<= 572 °FInjection
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 - 100 °C
@Time 14400 sec
176 - 212 °F
@Time 4.00 hour
Moisture Content <= 0.10 %<= 0.10 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4567 / 280367

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.