MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Nabaltec NABALOX® NO 784 Super-reactive, Monomodal Aluminas
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: NABALOX® aluminum oxide has a number of advantages including
  • low sintering temperature
  • wide sintering range
  • flexible processing
  • high sintered densities high wear and impact resistance
  • electrical insulation
  • high mechanical strength
  • high temperature properties
  • dimensional accuracy
  • optimized chemical resistance

Chemical industry, Glass industry, Corundum, Refractory industry, Household ceramics, Electroceramics, Engineering ceramics

Information provided by Nabaltec

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³Green density
 3.86 g/cc0.139 lb/in³Sintered density
Particle Size 0.50 µm0.50 µmprimary
 0.80 µm0.80 µmMedian
Specific Surface Area 7.0 m²/g7.0 m²/g
 
Thermal PropertiesMetricEnglishComments
Shrinkage 19 %19 %Linear
 
Processing PropertiesMetricEnglishComments
Sintering Temperature 1600 °C2910 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 95 %95 %alpha-Al2O3 content
 99.8 %99.8 %
Fe2O3 0.030 %0.030 %
Na2O 0.10 %0.10 %
SiO2 0.030 %0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott Sapphire Optical Window
Sapco 99.9% Aluminum Oxide
Morgan Advanced Ceramics Vitox® AMC Alumina Matrix Composite Aluminum Oxide Ceramic
Morgan Advanced Ceramics Deranox™ 999 Mac-A999R Aluminum Oxide Ceramic
China-Yixing Longly Refractories ZTA (20%ZrO2) Zirconia Toughened Alumina Composite Ceramic

CNABAL96 / 203689

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.