MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese Celanex® 5206HG PET, 15% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 20% Glass Reinforced

Material Notes: Celanex 5206HG is a 15% glass-filled polyester featuring super high surface gloss and high flow for long flow channels. A typical application is oven handles.

30% glass-fiber, improved impact

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 95.0 MPa13800 psi5mm/min; ISO 527-2/1A
Elongation at Break 1.8 %1.8 %5mm/min
Tensile Modulus 6.40 GPa928 ksi50mm/min; ISO 527-2/1A
Flexural Strength 135 MPa19600 psiISO 178
Flexural Modulus 6.30 GPa914 ksiISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²2.14 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.470 J/cm²2.24 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 180 °C356 °FISO 75-1, -2
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release
Techmer ES HiFill FR® PET GF15 IM FR X 15% Glass Filled
BASF Petra® 110 BK-112 15% Glass Filled PET
LG Chemical Lupox® SG5200 PBT+PET+GF20%
Reliance Industries PET - 35% Glass filled

PHCQ075A / 183204

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.