MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Fibre Glast 70 Styrene Monomer
Categories: Fluid; Solvent

Material Notes: #70 Styrene Monomer is the recommended and accepted thinner for polyester resins and gel coats. Most gel coats can be thinned 2-5% to make them suitable for heavy spray equipment or other special purposes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity >= 0.908 g/cc>= 0.908 g/ccCos-Mar Method
 
Descriptive Properties
Aldehyde (wt. %)Nil (Typical)ASTM D2119-87
Benzene (ppm)<1.0 (Typical)Cos-Mar Method
Color (Pt. Co.)4 (Typical)ASTM D1209-84
Ethylbenzene (ppm)70 (Typical)Cos-Mar Method
Inhibitor13 (Typical)ASTM D2120-87
Peroxides (wt. %)<0.001 (Typical)ASTM D2340-82
Polymer (ppm)2 (Typical)ASTM D2121-90
Purity (wt. %)99.93 (Typical)ASTM D3789-89
Toluene (ppm)<1.0 (Typical)Cos-Mar Method
Total Chlorides (wt. %)0.0004 (Typical)Cos-Mar Method
Total Sulfur (wt. %)Nil (Typical)Cos-Mar Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WFIBRE100 / 104537

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.