MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow INNATE™ TH60 Resin
Categories: Polymer; Thermoplastic

Material Notes: Product Description: INNATE™ TH60 precision packing resin is designed for exceptional toughness in combination with sealing performance while also delivering robust processability. It has exceptional low-temperature toughness and flex-crack resistance, making it a versatile resin that can meet the needs of demanding end-use applications.

Availability: Asia Pacific; Europe; Latin America; North America

Agency Ratings: EU 2011/10/EC; FDA FCN 424

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.914 g/ccASTM D792
Melt Flow 0.85 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 23.8 lb (f)
Film Tensile Strength at Yield, MD 1210 psiASTM D882
Film Tensile Strength at Yield, TD 1230 psiASTM D882
Film Elongation at Break, MD 580 %ASTM D882
Film Elongation at Break, TD 660 %ASTM D882
2% Secant Modulus 21000 psiMD; ASTM D8822
 24500 psiTD; ASTM D8822
Puncture Energy 92.9 in-lb
Elmendorf Tear Strength MD 520 gASTM D1922
Elmendorf Tear Strength TD 820 gASTM D1922
Dart Drop Test 2100 gMethod A; ASTM D1709
Film Tensile Strength at Break, MD 7430 psiASTM D882
Film Tensile Strength at Break, TD 7530 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 253 °F
Vicat Softening Point 208 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 14 %ASTM D1003
Gloss 51 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 433 °F
Blow-up Ratio (BUR) 2.5
 
Descriptive Properties
Film Puncture Resistance318 ft-lb/in3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF550 / 311243

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.