MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plaskolite Optix® PL-25 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Grade, Molded

Material Notes: Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line.

Data provided by the manufacturer, Plaskolite, Inc.

Key Words: PMMA; Polymethyl Methacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Water Absorption 0.30 %ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm48 hrs; ASTM D955
Melt Flow 2.0 g/10 minCondition I; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 95Method A; ASTM D785
Tensile Strength, Yield 72.0 MPaASTM D638
Tensile Modulus 3.00 GPaASTM D638
Flexural Yield Strength 110 MPaASTM D790
Izod Impact, Notched 0.400 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.7
@Frequency 60 Hz
ASTM D150
Dielectric Strength 18.0 kV/mmASTM D149
Dissipation Factor 0.050
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 54.0 µm/m-°C
@Temperature -18.0 - 38.0 °C
ASTM D696
Specific Heat Capacity 1.50 J/g-°C
Thermal Conductivity 0.200 W/m-KASTM C177
Melting Point 157 °CFlow temperature; ASTM D569
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °CASTM D648
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49
@Wavelength 589.3 nm
nD; ASTM D542
Transmission, Visible 92 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plaskolite West Optix® CA - 41 FDA General Purpose Acrylic Resin
Röhm Acrylite® AR Acrylic Sheet, Abrasion Resistant
Trinseo Plexiglas® MI7 Acrylic
LG Chemical Lupoy 1302EP-30 Polycarbonate Resin
LG Chemical Lupoy 1201-22 Polycarbonate Resin

PPLAS0 / 56273

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.