MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 2A25 Co-Extruded Multi-Polymer Protect Tapes
Categories: Polymer; Adhesive

Material Notes: 3M™ Co-Extruded Multi-Polymer Protective Tapes have a medium-tack adhesive system to help provide temporary protection for a variety of surface protection applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milASTM D3652
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 2.00 MPa290 psiASTM D882
Elongation at Break 600 %600 %ASTM D882
Peel Strength 0.0657 kN/m0.375 pliAdhesion to Steel; ASTM D3330
 
Descriptive Properties
Adhesive TypeAcrylic
AppearanceClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 25A87 Co-Extruded Polyethylene Protective Tapes
3M 25A88 Co-Extruded Polyethylene Protective Tapes
3M 25A29 Co-Extruded Polyethylene Protective Tapes
3M 25A26 Co-Extruded Polyethylene Protective Tapes
3M 25A25 Co-Extruded Polyethylene Protective Tapes

PMM34291 / 169038

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.