MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sumitomo Bakelite SUMILITERESIN® PR-50590 I Powder phenolic resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: SUMILITERESIN® PR-50590 I is a powder form phenolic resin with good grinding properties and good processability in the production of grinding wheels. It is designed for cold molding and semi-hot molding processes. SUMILITERESIN® PR-50590 I is a middle flow type and it has hexamine content of about 9%. Use of this resin will increase the ease of handling for coated grain. This product is also prefereable for heavy duty grinding wheels and long life wear.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 75 µm75 µmmax 1%
 
Thermal PropertiesMetricEnglishComments
Melting Point 88.0 - 98.0 °C190 - 208 °F
 
Processing PropertiesMetricEnglishComments
Gel Time 1.42 - 2.08 min
@Temperature 150 °C
1.42 - 2.08 min
@Temperature 302 °F
 
Descriptive Properties
AppearanceWhite-yellow powder
Flow Distance20-40mm, 125°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUMIT580 / 194385

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.