MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik VESTAKEEP® i2 UFP10 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP® i2 UFP10 is an unreinforced, medium-viscosity, natural colored polyether ether ketone (PEEK) ultra-fine powder. VESTAKEEP® i2 UFP10 is especially designed for long term implantable medical devices. The semi-crystalline polymer is designed for high biocompatibility and superior mechanical, thermal and chemical resistance.
Dry properties listed below
Industrial Sector: Medical Devices
Processing: Press and sintering, Coating
Delivery form: Powder
Optics: X-ray transparent
Resistance to: Heat (thermal stability), Hydrolysis / hot water
Conformity: Biocompatibility, Medical application
Additives: Unfilled
Special Characteristics: Semi-crystalline, Low viscosity, Sterilizable
Regulatory: US Pharmacopeia Class VI conformity
Color: Natural color
Delivery form: Ultrafine powder (UFP)
Chemical Resistance: Acid resistance, Alkali resistance, Solvent resistance, Grease resistance, Hydrolytically stable, Oil resistance, Oxidation resistance, General chemical resistance

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 0.230 g/cc0.00831 lb/in³EN ISO 60
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Particle Size 11.0 µm11.0 µmD50; ISO 13320, DIN ISO 8130-13
 <= 55.0 µm<= 55.0 µmISO 13320, DIN ISO 8130-13
Melt Flow 70.0 g/10 min
@Load 5.00 kg,
Temperature 380 °C
70.0 g/10 min
@Load 11.0 lb,
Temperature 716 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiISO 527
Tensile Strength, Yield 100 MPa14500 psiISO 527
Elongation at Break 30.0 %30.0 %Nominal; ISO 527
Elongation at Yield 5.00 %5.00 %ISO 527
Tensile Modulus 3.70 GPa537 ksiISO 527
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 340 °C644 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °FISO 75-1/-2
Vicat Softening Point  310 °C
@Load 5.10 kg
590 °F
@Load 11.2 lb
50 K/h; ISO 306
 335 °C
@Load 1.02 kg
635 °F
@Load 2.25 lb
50 K/h; ISO 306
Flammability, UL94 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
IEC 60695-11-10
 
Descriptive Properties
ColorNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7863 / 324995

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.