MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NextGen Adhesives P907-12 Fiber Optic Adhesive
Categories: Polymer; Adhesive

Material Notes: Description: NGAC P907-12 is a rapid curing, low viscosity, heat cured epoxy adhesive system that is specifically formulated for use in the fiber optic industry.

Advantages and Applications: Uses include bonding fiber optic bundles, potting glass fiber bundles and termination of single mode and multimode fiber optic connectors. NGAC P907-12 is a low viscosity mixture that ensures exceptional wicking and wetting of the fibers, along with superior adhesion strength. Additionally, it provides excellent thermal and moisture resistance.

Information Provided by Nextgen Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
Solids Content 100 %100 %
Viscosity 2000 cP2000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 85>= 85
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 175 °C347 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 115 °C239 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.561.56
 
Processing PropertiesMetricEnglishComments
Cure Time  1.00 min
@Temperature 150 °C
0.0167 hour
@Temperature 302 °F
 5.00 min
@Temperature 125 °C
0.0833 hour
@Temperature 257 °F
 15.0 min
@Temperature 100 °C
0.250 hour
@Temperature 212 °F
Pot Life 60 - 120 min60 - 120 min
 
Descriptive Properties
ColorReddish Brown
Mix Ratio by Weight (R/H)100/10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP42HT-2LTE Two Component Epoxy
Master Bond EP21TCHT-1 Thermally Conductive, Heat Resistant Epoxy Compound

PNEXT004 / 90251

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.