MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Edgetek® PC-30GF/000 BLACK Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D792
Filler Content 30 %Glass Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0020 - 0.0050 cm/cm
@Thickness 3.18 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 117 MPa5.1 mm/min; ASTM D638
Elongation at Break 3.0 - 4.0 %ASTM D638
Tensile Modulus 8270 MPa5.1 mm/min; ASTM D638
Flexural Strength 186 MPa1.3 mm/min; ASTM D790
Flexural Modulus 7310 MPa1.3 mm/min; ASTM D790
Izod Impact, Notched 130 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 142 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °CUnannealed; ASTM D648
 
Descriptive Properties
FeaturesAmorphous
 Good Dimensional Stability
 Good Toughness
FormsPellets
Generic MaterialPC
Generic NamePolycarbonate (PC)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAppliance Components
 Appliances
 Automotive Applications
 Automotive Interior Parts
 Business Equipment
 Consumer Applications
 General Purpose
 Housings

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® PC-30CF/000 BLACK Polycarbonate (PC)
PTS Tristar® PC-30GF 30% Glass Reinforced Polycarbonate With Release
Avient Edgetek® PC-20GF/000 Polycarbonate (PC)
Avient LubriOne™ PC-20GF/15T Polycarbonate (PC)
Covestro Bayblend® FR3000 PC/ABS Blend

PH0POL0125 / 144694

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.