MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Marco Polo MARPOL COPP 20.NB Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: MARPOL CoPP 20.NB is a high melt flow rate impact copolymer polypropylene for injection molding applications. It offers very high impact resistance and good stiffness. This resin meets the requirements of the U.S. FDA as specified in 21 CFR 177.1520.

Processing Method: Injection molding

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.894 g/cc0.0323 lb/in³ASTM D792
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 6767ASTM D785
Tensile Strength at Break 16.0 MPa2320 psi2 in/min; ASTM D638
Tensile Strength, Yield 21.0 MPa3050 psi2 in/min; ASTM D638
Elongation at Break >= 300 %>= 300 %2 in/min; ASTM D638
Elongation at Yield 7.9 %7.9 %2 in/min; ASTM D638
Flexural Modulus 0.910 GPa132 ksi0.01; ASTM D 790A
Izod Impact, Notched  0.908 J/cm
@Temperature -20.0 °C
1.70 ft-lb/in
@Temperature -4.00 °F
ASTM D256A
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C180 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C118 °FASTM D648
Vicat Softening Point 143 °C289 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss 83 %83 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARCO025 / 283622

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.