MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Pressure Seal 13525 Chlorobutyl
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 13525 is 50 durometer white colored Chlorobutyl elastomer.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 AA 510 A13 EA14 F17; 3 AA 510 B33 EA14 F17; 2 BA 510 F17

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5151
 49
@Treatment Temp. 70.0 °C,
Time 252000 sec
49
@Treatment Temp. 158 °F,
Time 70.0 hour
Heat Aged
 55
@Treatment Temp. 100 °C,
Time 252000 sec
55
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
 59
@Treatment Temp. 100 °C,
Time 252000 sec
59
@Treatment Temp. 212 °F,
Time 70.0 hour
Distilled water aged
Tensile Strength 8.239 MPa1195 psi
 7.7449 MPa
@Treatment Temp. 70.0 °C,
Time 252000 sec
1123.3 psi
@Treatment Temp. 158 °F,
Time 70.0 hour
Heat Aged
 8.9397 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
1296.6 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
Elongation, Ultimate 920 %920 %
 770.1 %
@Treatment Temp. 100 °C,
Time 252000 sec
770.1 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
 850.1 %
@Treatment Temp. 70.0 °C,
Time 252000 sec
850.1 %
@Treatment Temp. 158 °F,
Time 70.0 hour
Heat Aged
100% Modulus 0.917 MPa133 psi
Tear Strength 21.4 kN/m122 pliDie B
Compression Set  28.5 %
@Treatment Temp. 70.0 °C,
Time 79200 sec
28.5 %
@Treatment Temp. 158 °F,
Time 22.0 hour
Plied
 33.2 %
@Treatment Temp. 70.0 °C,
Time 79200 sec
33.2 %
@Treatment Temp. 158 °F,
Time 22.0 hour
Solid
 75.3 %
@Treatment Temp. 100 °C,
Time 79200 sec
75.3 %
@Treatment Temp. 212 °F,
Time 22.0 hour
Solid
 78.8 %
@Treatment Temp. 100 °C,
Time 79200 sec
78.8 %
@Treatment Temp. 212 °F,
Time 22.0 hour
Plied
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -43.9 °C-47.0 °F
Shrinkage 9.2 %
@Treatment Temp. 100 °C,
Time 252000 sec
9.2 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, Distilled water aged
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRESL090 / 318300

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.