MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Honeywell BF3 High Purity Gas Specifications
Categories: Fluid

Material Notes: Boron Trifluoride

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.00300 g/cc0.000108 lb/in³Gas at STP
 0.591 g/cc0.0214 lb/in³Critical
 1.57 g/cc0.0567 lb/in³Liquid at BP
 1.68 g/cc0.0607 lb/in³Liquid at MP
Molecular Weight 67.81 g/mol67.81 g/mol
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 49.84 bar37380 torr
Critical Temperature -24.60 - -24.57 °C-12.28 - -12.22 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point -128.37 °C
@Pressure 0.101 MPa
-199.07 °F
@Pressure 14.7 psi
Boiling Point -73.56 °C
@Pressure 0.101 MPa
-100.4 °F
@Pressure 14.7 psi
 
Descriptive Properties
Assay>99.5%DTM 3-4
Content<0.001%Sulfate
 <0.002%SO2
 <0.03%SiF4
 <0.4%Air
Entropy253.81 kJ/(g-mol)(°C)298.15°K
Heat of Fusion4.238 kJ/g--mol
Heat of Reaction102.55 kJ/g-molin excess water
Heat of Vaporization18.56 kJ/g-mol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHONWL129 / 179674

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.