MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik Sanicro 26Mo logging cable Precision Wire
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Sanicro 26Mo is a high­alloy austenitic stainless steel for service in highly corrosive conditions in oil and gas environments. The grade is characterized by:
  • Very good resistance to stress corrosion cracking (SCC) in H S, chloride and CO2 environments
  • Very good resistance to pitting in chloride-containing environments because of its high PRE* value of 43 minimum
  • Very good resistance to general corrosion
  • High mechanical strength and correspondingly high breaking loads
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 1585 MPa>= 229900 psiSlicklines
 >= 1655 MPa>= 240000 psiLogging cable armor wire
Tensile Strength, Yield  >= 1350 MPa
@Strain 0.2 %
>= 196000 psi
@Strain 0.2 %
Slicklines
 >= 1410 MPa
@Strain 0.2 %
>= 204000 psi
@Strain 0.2 %
Logging cable armor wire
Modulus of Elasticity 185 GPa26800 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 - 100 °C
7.78 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 10.0 W/m-K69.4 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.020 %<= 0.020 %
Chromium, Cr 20.5 %20.5 %
Copper, Cu 0.80 %0.80 %
Iron, Fe 45.9 %45.9 %As Balance
Manganese, Mn 0.80 %0.80 %
Molybdenum, Mo 6.3 %6.3 %
Nickel, Ni 25 %25 %
Nitrogen, N 0.20 %0.20 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.40 %0.40 %
Sulfur, S <= 0.0050 %<= 0.0050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV217 / 19111

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.