MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) AvaSpire® AV-722 Polyaryletherketone (PAEK), Low melt flow for extrusion and injection molding
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Unreinforced

Material Notes: AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formulated for applications requiring high chemical resistance and mechanical strength along with low moisture absorption and good barrier properties. These and other properties make this resin well-suited for applications in healthcare, transportation, electronics, chemical processing and other industries.

- Beige: AvaSpire® AV-722 BG 20

Markets/Uses: Aircraft / Mechanical & Structural Applications / Cable Ties; Aircraft / Mechanical & Structural Applications / Engine Components; Aircraft / Mechanical & Structural Applications / Handles; Aircraft / Mechanical & Structural Applications / Seals; Aircraft / Mechanical & Structural Applications / Stock Shapes for Prototyping; Aircraft / Mechanical & Structural Applications / Thermal Acoustical Insulation Blankets and Burnthrough Protection Layers; Aircraft / Mechanical & Structural Applications / Thin Films and Tapes; Aircraft / Mechanical & Structural Applications / Tubing; Automotive / Fuel Systems / Filter Housings; Automotive / Fuel Systems / Fuel Rails; Automotive / Fuel Systems / Quick Connects; Automotive / Fuel Systems / Sheet and Film; Automotive / Mechanical & Structural Parts / Gears; Automotive / Mechanical & Structural Parts / Poppets; Films / High Temperature Films / Cable Ties; Films / High Temperature Films / Engine Components; Films / High Temperature Films / Handles; Films / High Temperature Films / Seals; Films / High Temperature Films / Thermal Acoustical Insulation Blankets and Burnthrough Protection Layers; Films / High Temperature Films / Thin Films and Tapes; Films / High Temperature Films / Tubing; Healthcare / Medical Devices / Case Handles and Brackets; Healthcare / Medical Devices / Dental Instruments; Healthcare / Medical Devices / Medical Pump Seals; Healthcare / Medical Devices / Medical Reusable; Healthcare / Medical Devices / Medical/Healthcare Applications; Healthcare / Medical Devices / Orthopedics; Healthcare / Medical Devices / Packaging, Rigid Medical; Healthcare / Medical Devices / Sizing Trials; Healthcare / Medical Devices / Surgical Instruments; Oil & Gas / Down Hole / Back-Up Seal Rings; Oil & Gas / Down Hole / Bushings and Bearings; Oil & Gas / Down Hole / Compressor Plates; Oil & Gas / Down Hole / Compressor Rings; Oil & Gas / Down Hole / Down Hole Connectors; Oil & Gas / Down Hole / Electrical Connectors; Oil & Gas / Down Hole / Flexible Riser/Umbilical; Oil & Gas / Down Hole / Labyrinth Seals; Oil & Gas / Down Hole / Motor End Plate; Oil & Gas / Down Hole / Poppets; Oil & Gas / Down Hole / Sucker Rod Guides

Applications: Aircraft Applications; Automotive Applications; Electrical/Electronic Applications; Film; Fuel Lines; Gears; Medical/Healthcare Applications; Oil/Gas Applications; Seals

Features: Chemical Resistant; Ductile; Flame Retardant; Good Dimensional Stability; Good Impact Resistance; High Heat Resistance

Injection notes: Back Pressure: Minimum

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccASTM D792
Water Absorption 0.10 %
@Time 86400 sec
ASTM D570
Viscosity 450 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm
@Thickness 3.18 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.012 - 0.014 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 400 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 95ASTM D785
Tensile Strength 89.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 91.0 MPaType 1A, 50 mm/min; ISO 527-2
Elongation at Break 25 %50 mm/min; ASTM D638
 25 %Type 1A, 50 mm/min; ISO 527-2
Elongation at Yield 4.5 %Type 1A, 50 mm/min; ISO 527-2
 5.0 %50 mm/min; ASTM D638
Tensile Modulus 3700 MPa50 mm/min; ASTM D638
 3900 MPa1 mm/min, Type 1A; ISO 527-2
Flexural Strength 138 MPaISO 178
 141 MPaASTM D790
Flexural Modulus 3700 MPaASTM D790
 3800 MPaISO 178
Compressive Strength 112 MPaASTM D695
Poissons Ratio 0.43ASTM E132
Shear Strength 79.0 MPaASTM D732
Izod Impact, Notched 80.0 J/mASTM D256
Izod Impact, Unnotched NBASTM D256
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) NBISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.10e+17 ohm-cmASTM D257
Surface Resistance >= 1.90e+17 ohmASTM D257
Dielectric Constant 3.06
@Frequency 1e+6 Hz
ASTM D150
 3.12
@Frequency 60 Hz
ASTM D150
Dielectric Strength 19.0 kV/mm
@Thickness 3.00 mm
ASTM D149
 170 kV/mm
@Thickness 0.0500 mm
Amorphous Film; ASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D150
 0.0040
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 45.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
Specific Heat Capacity 1.41 J/g-°C
@Temperature 50.0 °C
ASTM C351
 1.97 J/g-°C
@Temperature 200 °C
ASTM C351
Thermal Conductivity 0.220 W/m-KASTM C177
Melting Point 340 °CPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 161 °C
@Thickness 3.20 mm
Annealed; ASTM D648
Glass Transition Temp, Tg 150 °CDSC
Oxygen Index 40 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 354 °C
Middle Barrel Temperature 366 °C
Front Barrel Temperature 371 °C
Nozzle Temperature 374 °C
Mold Temperature 177 - 204 °C
Drying Temperature 149 °C
@Time 14400 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBeige
FormsPellets
Injection RateFast
ProcessingExtrusion Blow Molding; Fiber (Spinning) Extrusion; Film Extrusion; Injection Blow Molding
 Injection Molding; Machining; Profile Extrusion; Thermoforming; Wire & Cable Extrusion
Screw Compression Ratio2.5:1.0 to 3.5:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4154 / 279954

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.