MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Meyors Chemical Rubber Accelerator MBT (M) Granule
Categories: Other Engineering Material

Material Notes: Product Code: MSHQD -AC001-00GT
Chemical Name: 2-mercaptobenzothiazole
Trade Name: Rubber Accelerator MBT (M)
CAS No.: 149-30-4
Molecular Formula: C7H5NS2

Typical Properties: It is yellow granule with little osmyl and taste bitter. The density is 1.42-1.52.it is soluble in ethyl acetate, ethanol, solution of NaOH and Na2CO3, insoluble in benzene, water and gasoline. Lower explosion limit is 21g/m3.

Recommended Applications: In NR compounds, MBT based vulcanization systems exhibit less reversion upon overcure than other systems. Vulcanizate obtained with MBT tend to have a relatively low modulus but very good aging properties. To achieve a faster cure and a higher modulus. MBT can be boosted by the use of secondary accelerators, such as ZBEC, ZDEC, TMTD or DPG. For the vulcanization of EPDM or IIR rubbers, MBT is a well established component of many existing vulcanization systems. MBT also finds application in latex form cure systems. It is non-staining and non-discoloring.

Information provided by Meyors Chemical INC Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.400 - 0.440 g/cc
 0.560 - 0.600 g/ccCompacted
Density 1.42 - 1.52 g/cc
Molecular Weight 167.26 g/mol
Ash <= 0.50 %
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 170 °CInitial
 
Descriptive Properties
AppearanceLight yellow powder
Assay content>95%
Loss on drying<0.5%
Strength of grain0.8-2.5 N

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMEYORS004 / 316586

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.