MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Epoxies, Etc 20-2028 Foam in Place Rigid Polyurethane Foam
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: 20-2028 is a light weight, two component, closed cell, liquid urethane foaming resin system. It produces a foam which will provide moisture resistance, high impact strength, better flow and fast mold cycle rates. The density is 11 pounds per cubic foot. 20-2028 is a water blown rigid foam that does not contain any hydrochlorofluorocarbon (HCFC). It is also safer to use since it does not utilize MOCA or TDI. 20-2028 has been formulated for ease in handling with a convenient 1:1 mix ratio. Castings can be hand poured or machine dispensed.

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccMixed
Viscosity 250 cPResin
 1400 cPResin
Storage Temperature 21.0 - 29.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 38
Tensile Strength 60.0 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.25
@Frequency 1e+6 Hz
Dissipation Factor 0.0050
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0400 W/m-K
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -50.0 °C
 
Descriptive Properties
ColorTan
Cream Time60 sec
Demolding Time10 min
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX009 / 316686

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.