MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Veradel® 3100P Polyethersulfone (PESU), Coarse powder for coatings
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Coarse powder for coatings, medium viscosity

Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other solid particles. The grades differ by their molecular weights, with 3000P the highest and 3600P the lowest. There is a direct correlation between molecular weight and solution viscosity.

PESU offers excellent toughness and outstanding hydrolytic resistance. It resists attack from steam, boiling water, and mineral acids. Cast films or coatings of PESU are transparent and have additional desirable properties including long term thermal stability, excellent metal adhesion and formability and inherent flame resistance.

Typical applications include high-temperature coating formulations, membranes, advanced high-temperature composites, and specialty adhesives.

This grade was formerly marketed as Gafone™ PESU

Markets/Uses: Membranes / Membranes / Biomedical; Membranes / Membranes / Bioprocessing; Membranes / Membranes / Food and Beverage Processing; Membranes / Membranes / Industrial Process Separations; Membranes / Membranes / UF/MF Low Pressure Water Filtration; Membranes / Membranes / Waste Treatment; Membranes / Membranes / Water Purification

Applications: Adhesives; Coating Applications; Compounding; Film; Membranes

Features: Acid Resistant; Chemical Resistant; Creep Resistant; Flame Retardant; Food Contact Acceptable; Good Adhesion; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Molecular Weight; High Tensile Strength; Hydrolysis Resistant; Low Flow; Medium Rigidity

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ASTM D792
Water Absorption 0.60 %
@Time 86400 sec
0.60 %
@Time 24.0 hour
ASTM D570
Viscosity 800 cP800 cPSolution Viscosity; ASTM D445
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 49.0 µm/m-°C27.2 µin/in-°FASTM D696
Glass Transition Temp, Tg 220 °C428 °FASTM E1356
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsGranules; Powder
ProcessingCast Film; Coating; Solution Processing
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4587 / 280387

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.