MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Asahi Kasei Stylac™ IC24 ABS Polymer, Electrically Conductive
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes:

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D955
Melt Flow 12 g/10 min
@Load 9.99 kg,
Temperature 220 °C
12 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 79.0 MPa11500 psi50mm/min; ISO 527-1
Flexural Strength 114 MPa16500 psi2mm/min; ISO 178
Flexural Modulus 2.80 GPa406 ksi2mm/min; ISO 178
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 ohm-cm1000 ohm-cmoriginal
Surface Resistance 10000 ohm10000 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 101 °C214 °FISO 75-1,2
Vicat Softening Point 106 °C
@Load 5.10 kg
223 °F
@Load 11.2 lb
ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Stylac™ IC10N ABS Polymer, Electrically Conductive
Carlisle 201LD Carbon-Carbon Composite
Asahi Kasei Stylac™ 789 ABS Polymer, Heat Resistant
A. Schulman ComAlloy Comshield® 220 ABS, Electrically Conductive - Carbon Black Filled

PASAHI8283 / 221307

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.