MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Taiwan PU TPUA-15-AM85I TPU Hot Melt, Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Key features:
  • High adhesion strength to all kinds of material
  • Good flexibility at low temperature
  • High extensibility
  • Good tensile strength
  • Fast crystallization rate
Application: This series of TPU is designed as hot melt adhesive. They are suitable for the following applications: Hot-Melt Adhesive Film, Seam Tape, Textile Lamination, Fabric Coatings, Heat Sealable Fabrics, Low Temperature Lamination Sheets, Heat Transfer Lamination, Automotive Industry, Woodworking and others

Features: TPU for hot melt adhesive performs good bonding strength for TPU, Nylon, PVC, Leather, Polyester, Fabrics, etc.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 10 - 20 g/10 min
@Load 2.16 kg,
Temperature 150 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92 - 98
 
Thermal PropertiesOriginal ValueComments
Softening Point 60.0 - 70.0 °CFlowing
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 minTack Free Time

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTAIWPU117 / 305847

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.