MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Thermoset™ SC-303 Silicone Encapsulant, Flame Retardant
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Lord SC-303 is a two component silicone elastomer that provides excellent thermal conductivity, while retaining the other desirable properties associated with silicones. It is a low viscosity, easily pourable liquid that is ideally suited for electrical/electronic potting applications. It has excellent high heat performance, thermal shock resistance, and improved coefficient of expansion.

Lord SC-303 has been formulated for flame retardancy and is an Underwriters Laboratories recognized material under the Components-Plastics classification as 94V-0 at 0. 250 inches.

Lord SC-303 resin is white and the hardener is gray. These colors act as mix indicators. When thoroughly mixed, SC-303 is lighter gray.

Lord SC-303 is addition curing. It will not depolymerize when heated in confined spaces as do many condensation curing silicones. As with all silicones, SC-303 generates no exotherm as it cures. It also exhibits low shrinkage and stress on components as it cures. Lord SC-303's cure may be accelerated with elevated temperature.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.10 g/ccSTM 2
Water Absorption 0.050 %ASTM D570-81
Viscosity 7000 cP
@Temperature 25.0 °C
STM 1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45ASTM D2240
Tensile Strength, Yield 170 psiASTM D412
Elongation at Yield 90 %ASTM D412
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.80e+15 ohm-cm
@Temperature 25.0 °C
ASTM D257
Dielectric Constant 4.2
@Frequency 1e+6 Hz,
Temperature 25.0 °C
ASTM D150
Dielectric Strength 440 V/milASTM D149
Dissipation Factor 0.00040
@Frequency 1e+6 Hz,
Temperature 25.0 °C
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 163.33 µm/m-°CCalculated from Volume CTE; ASTM D864
Thermal Conductivity 0.800 W/m-KHot Disc Transient Method
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 V-0
@Thickness >=6.35 mm
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 - 15.0 min
@Temperature 100 °C
 24.0 hour
@Temperature 25.0 °C
 25.0 - 30.0 min
@Temperature 70.0 °C
Pot Life 50 min
@Temperature 25.0 °C
100 grams
Shelf Life 9.00 Month
@Temperature 25.0 °C
 
Descriptive Properties
AppearanceGrayHardener
 Light GrayMixed
 WhiteResin
Mix Ratio1:1by weight, by volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lord Adhesives CoolTherm™ SC-320 Thermally Conductive Silicone Encapsulant
Lord Adhesives CoolTherm™ SC-6709/6730 Silicone encapsulant system
Lord Adhesives CoolTherm™ SC-6710/6731 Silicone Resin System
Lord Adhesives CoolTherm™ SC6711/6730 Silicone Encapsulant
Lord Adhesives CoolTherm™ SC6711/6731 Silicone Encapsulant

PLORD065 / 86073

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.