MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Syncon® ISO Grade 32 Turbine Oil
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Syncon Turbine Oil is a premium quality, synthetic lubricant developed for use in land-based gas turbines operating over a wide temperature range, where the manufacturer calls for a synthesized hydrocarbon (SHC) or PAO-based turbine oil. Syncon Turbine Oil is formulated with synthetic polyalphaolefin (PAO) base oils and select additives to provide outstanding performance and protection in gas turbines. It has outstanding oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It has high load-carrying capacity to protect against wear. It protects system components against rust and corrosion, and is resistant is excessive foam buildup that can interfere with proper lubrication. It has a high viscosity index and a very low pour point for use over a wide temperature range.

Applications:

  • Land-based gas turbines
Syncon Turbine Oil meets the requirements of the following OEM specification:
  • Solar Turbines ES 9-224, Revision W, Class I (Synthesized Hydrocarbon) Turbine Oil
Features/Benefits:
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • Excellent low-temperature fluidity
  • High viscosity index and very low pour point for use over a wide temperature range
  • Low volatility for lower oil consumption and less makeup oil
  • Protects against wear
  • Protects against rust and corrosion
  • Good foam resistance
  • Extended service intervals compared with conventional mineral oil-based lubricants

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.841 g/cc
Density 7.00 lb/gal
Viscosity Measurement 136Index
Saybolt Viscosity at 100°F 164 SUS
Saybolt Viscosity at 210°F 46.3 SUS
Kinematic Viscosity at 40°C (104°F) 32 cSt
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
Oxidative Stability 26.67 hourRPVOT; ASTM D2272
ASTM Color 0.50ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.36[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.400 mmScar Diameter; ASTM D4172
 
Thermal PropertiesOriginal ValueComments
Pour Point -57.0 °C
Flash Point 254 °CCOC
 
Descriptive Properties
Copper Corrosion1aASTM D130
Demulsibility10 minutes to passASTM D1401
FZG Scuffing Test>8 Failure Load StageASTM D5182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5272 / 198525

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.