MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Tabriz HD 5218UA High Density Polyethylene Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: HD5218UA is high density polyethylene copolymer containing butene-1(C4) as comonomer. It is suitable for thin wall injection molding applications. HD5218UA has high warpage resistance, high flow, fast cycling injection molding, UV stabilized. This grade has food contact approval. Applications: general purpose injection molding with outdoor & indoor applications.

Information provided by Tabriz Petrochemical Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccASTM D1505
Brightness 60.0 %Whiteness Index; ASTM E313
Melt Flow 18 g/10 min
@Load 2.16 kg
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 20.0 MPaASTM D638
Elongation at Break 900 %ASTM D638
Charpy Impact, Notched 3.00 kJ/m²ASTM D6110
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 115 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Yellow Index -1.00 %ASTM E313
 
Descriptive Properties
Contamination (No.)5BP137

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 799 X 144652 G High Density Polyethylene (HDPE); ESD Protection - Permanently Static Dissipative - Preliminary Datasheet
Unipetrol PE HD LITEN® MB/ML 62 HDPE
Dow UNIVAL™ DMDD-6230 NT 7 High Density Polyethylene Resin (HDPE)
RheTech Products E204-01 High Density Polyethylene, Black
Westlake HM 5020 High Density Polyethylene

PTABRZ908 / 198219

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.