MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

CRG Industries Veriflex® Shape Memory Polymer Resin  (Unverified Data**)
Categories: Polymer; Thermoset

Material Notes: Veriflex® is a two-part, fully formable, thermoset shape memory polymer (SMP) resin system. Cured Veriflex has unique “shape memory” properties. When heated above its activation temperature (Tg), Veriflex changes from a rigid plastic to a flexible elastomer. In its elastic state, it can be twisted, pulled, bent, and stretched, reaching up to 200% elongation. If cooled while constrained in this new shape, the polymer hardens and can maintain its new shape. When heated, unconstrained, above its Tg, this polymer returns to the shape in which it was cured. This process can be repeated indefinitely without loss of the memory shape or degradation of the material.

Standard Veriflex resin is engineered with a Tg of 62 °C (144 °F). Uncured Veriflex resin has a low viscosity that makes it easy for RTM or VARTM processing and composite fabrication. Typical applications include customizable and reusable molds, toys, architectural applications, furniture, deployment mechanisms, containers, shipping and packaging, thermal sensors, and actuators.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 23.0 MPa3340 psiASTM D638
Elongation at Break 3.9 %3.9 %ASTM D638
Tensile Modulus 1.24 GPa180 ksiASTM D638
Flexural Strength 37.1 MPa5380 psiASTM D790
Flexural Modulus 1.24 GPa180 ksiASTM D790
Compressive Strength 32.4 MPa4700 psiASTM D695
Compressive Modulus 1.45 GPa210 ksiASTM D695
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.170 W/m-K
@Temperature 18.3 °C
1.18 BTU-in/hr-ft²-°F
@Temperature 65.0 °F
Maximum Service Temperature, Air 130 °C266 °F
Glass Transition Temp, Tg 62.0 °C144 °F

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCRG950 / 93190

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.