MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Domo TECHNYL® A 31T1 MZ40 PA66, 40% mineral fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Mineral Filled

Material Notes: Description: Flame retardant polyamide PA66, 40% mineral filled, heat stabilized, for injection molding.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: This flame retardant material offers very good dimensional stability and excellent Glow wire performance. This product is particularly recommended for electrical parts such as: low voltage distribution, protection systems, mini circuit breakers, fuse holders and terminal blocks. This product is available in grey.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.67 g/cc0.0603 lb/in³ISO 1183/A
Water Absorption 0.43 %
@Temperature 23.0 °C,
Time 86400 sec
0.43 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 77.0 MPa11200 psiISO 527 Type 1A
Elongation at Break 1.7 %1.7 %ISO 527 Type 1A
Tensile Modulus 6.90 GPa1000 ksiISO 527 Type 1A
Charpy Impact Unnotched 2.50 J/cm²11.9 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.220 J/cm²1.05 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243
Comparative Tracking Index 400 V400 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FISO 75/Af
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
1210
Oxygen Index 46.5 %46.5 %ISO 4589
Glow Wire Flammability Index  960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
ISO 60695-2-12
 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 270 - 275 °C518 - 527 °F
Front Barrel Temperature 285 - 290 °C545 - 554 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone285-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced
PlastiComp Complet® LCF40 - PA66 MT Nylon 66, 40% Long Carbon Fiber Reinforced, Impact Modified
PlastiComp Complet® LCF30 - PA66 Nylon 66, 30% Long Carbon Fiber Reinforced
DuPont Mobility and Materials Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA)
Avient Edgetek® AM-20CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced

PRHOD708 / 137939

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.