MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay XMTR50 (EF7313) Epoxy Resin System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: XMTR50 (EF7313) is a two part epoxy resin system developed specifically for the high rate manufacture of components using a High Pressure Resin Transfer Molding (HP-RTM) process. With HP-RTM molding equipment, XMTR50 (EF7313) can be used to manufacture components with a total cycle time of five minutes or less.

Features & Benefits:

  • Two part system
  • Low viscosity allowing for sub 30 sec injection times
  • Cure indicated by change of color (colorless to deep red)
  • Typically injected at 110 to 120°C (230 to 248°F), 40 to 80 bar (580.2 to 1160.3 psi) injection pressures
  • DMA E’ onset Tg 140°C after 3 minute cure at 120 and 130°C (248 and 266°F)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccHardener
 1.17 g/ccMixed
 1.20 g/ccResin
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 140 °CDMA E' onset Tg, 3 minutes at 120°C
 140 °CDMA E' onset Tg, 5 minutes at 120°C
 140 °CDMA E' onset Tg, 3 minutes at 130°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay MTM® 23 Vinyl Hybrid Prepreg
Henkel Loctite® 3563 Epoxy Snap Cure Underfill
Tra-Con Tra-Duct 925M01 Low Ion Snap Cure Silver-Filled Epoxy
Master Bond EP17HT-3 One component, snap-curing epoxy system
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting

PCYTED153 / 180455

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.