MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cadi MOLD-MOR™ 20
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: A Beryllium Copper Alloy with high thermal conductivity and moderate hardness.

Information provided by Cadi Company.

Key Words: UNS C17510
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.317 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 98
Tensile Strength at Break >= 88000 psi
@Thickness >=50.8 mm
 >= 90000 psi
@Thickness 25.4 - 50.8 mm
 >= 94000 psi
@Thickness <=25.4 mm
Tensile Strength, Yield >= 88000 psi
@Strain 0.5 %,
Thickness >=50.8 mm
 >= 90000 psi
@Strain 0.5 %,
Thickness 25.4 - 50.8 mm
 >= 94000 psi
@Strain 0.5 %,
Thickness <=25.4 mm
Modulus of Elasticity 19000 ksi
Poissons Ratio 0.267
Shear Modulus 7500 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 0.00000383 ohm-cm>45 %IACS, up to 3" diameter/any thickness
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1560 BTU-in/hr-ft²-°F
Melting Point 1885 - 1955 °F
Solidus 1885 °F
Liquidus 1955 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1450 °FBrazing
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 0.40 %
Copper, Cu 97.8 %
Nickel, Ni 1.8 %
 
Descriptive Properties
RMWA Class3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Brush Wellman Beryllium Copper Alloy 3 Strip; A-Dead Soft (TB00) Temper (UNS C17510)
Cadi MOLD-MOR™ 2
Materion Beryllium Copper Alloy 3 Forgings & Extrusions; A (TB00) Temper (UNS C17510)
Cadi MOLD-MOR™ 40
Cadi MOLD-MOR™ 30

NCADI08 / 15516

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.