  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® 3501-6 Epoxy Resin System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 3501-6 is an amine cured epoxy resin system supplied with unidirectional or woven carbon or glass fibers. Typical reinforcement is continuous AS4 carbon filaments. 3501-6 was developed to operate in a temperature environment of up to 350°F (177°C). AS4/3501-6 is recommended for general purpose structural applications.

Benefits and Features:

  • Service Temperature up to 350°F (177°C)
  • Damage-Resistant System
  • 350°F (177°C) Cure

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.265 g/cc
Viscosity 400 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 6.60 ksi
Tensile Modulus 615 ksi
Flexural Modulus 484 ksi
Compressive Strength 1.10 MPa
 1.95 MPaShear elongation to failure
Shear Strength 7.00 ksi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.1 µin/in-°F
@Temperature 23.9 - 72.8 °C
 24.4 µin/in-°F
@Temperature 71.1 - 121 °C
 33.3 µin/in-°F
@Temperature 121 - 177 °C
Glass Transition Temp, Tg 151 °C
@Temperature 177 °C,
Time >=21600 sec
wet
 210 °C
@Temperature 177 °C,
Time >=21600 sec
dry
 
Processing PropertiesOriginal ValueComments
Gel Time 4.00 - 10.0 min
@Temperature 177 °C
Shelf Life 0.300 Month
@Temperature 21.0 °C
 4.00 Month
@Temperature 4.00 °C
 12.0 Month
@Temperature -18.0 °C
 
Descriptive Properties
G1 C0.733 in-lb/in2Strain energy release rate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9118 / 322274

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.