MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Crosspolimeri EFRHATAN 75 P Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Efrhatan: is the trade-mark of our TPU.

Efrhatan 75 P: is a thermoplastic elastomeric polyurethane polyester plastified. This compound offer outstanding chemical and hydrolysis resistance. The material exhibit excellent physical-mechanical performances resulting in shoes and injected molding parts. Good processability and stability. Material to use on the production of technical parts. General purposes.

Certify: Suole e Stampaggio/Shoes and Injection

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccISO 1183
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575ISO 868
Tensile Strength 33.0 MPa4790 psiISO 527
Elongation at Break 680 %680 %ISO 527
Tear Strength >= 62.0 kN/m>= 354 pliambient; DIN 53515
Abrasion >= 38>= 38[mm³]; DIN 53516
 
Processing PropertiesMetricEnglishComments
Zone 1 175 °C347 °F
Zone 2 180 °C356 °F
Zone 3 180 °C356 °F
Zone 4 190 °C374 °F
Die Temperature 190 °C374 °F
Melt Temperature <= 200 °C<= 392 °F
Head Temperature 200 °C392 °F
Dry Time  3.00 hour
@Temperature 90.0 °C
3.00 hour
@Temperature 194 °F
 6.00 hour
@Temperature 90.0 °C
6.00 hour
@Temperature 194 °F
 
Descriptive Properties
Cold Flex-40°CISO 458
Exercise temperature70°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS026 / 294110

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.