MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Eclipse® SAE Grade 30 W Gas Engine Oil  (discontinued **)
Categories: Fluid; Lubricant

Material Notes: Phillips 66® Eclipse W Gas Engine Oil is a high-quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natural gas engines. It is particularly recommended for use in natural gas engines and dual-fuel engines burning sour gas or landfill gas. Eclipse W Gas Engine Oil is formulated to provide excellent resistance to oxidation and nitration, protect against piston scuffing and wear, and minimize the formation of engine sludge and piston deposits for good engine cleanliness. It has a high alkaline reserve (TBN) to protect engines operating under corrosive conditions, such as when burning sour gas, digester gas or landfill gas. Eclipse W is designed specifically for use in Waukesha gas engines, and has extensive field experience in Waukesha VHP GL turbocharged lean-burn engines. It also is recommended for use in other 4-stroke cycle natural gas engines that require a mid-ash gas engine oil containing 1 percent (nominal) sulfated ash.

Applications:

  • 4-stroke cycle gas and dual-fuel engines burning sour gas or landfill gas
  • 4-stroke cycle gas engines in wastewater treatment plants fueled by digester gas
  • 4-stroke cycle natural gas engines where the manufacturer specifies a mid-ash gas engine oil
Eclipse W is recommended for use in natural gas engines manufactured by:
  • Waukesha (VHP GL turbocharged, lean-burn engines, models 3521, 5115, 7042, 9390)
  • Cooper Superior
Features/Benefits:
  • Excellent resistance to oxidation and nitration
  • High dispersancy protects against engine sludge and varnish formation
  • Protects against scuffing and wear
  • Protects against rust and corrosion
  • High alkaline reserve to combat acidic combustion by-products when burning sour gas

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.879 g/cc
Density 7.32 lb/gal
Viscosity Measurement 104Index
Kinematic Viscosity at 40°C (104°F) 132 cSt
Kinematic Viscosity at 100°C (212°F) 14.1 cSt
Ash 0.94 %Sulfated; ASTM D874
ASTM Color 3.0ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Base Number 9.0ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -36.0 °C
Flash Point 240 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.079 %
Zinc, Zn 0.088 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON6048 / 210133

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.